EN10210 S355NH Carbon Steel Pipe
video

EN10210 S355NH Carbon Steel Pipe

EN 10210 S355NH pipes have become one of the most reliable and useful materials in various industries. It is used in different fields such as construction, manufacturing and mining.
Послати повідомлення
Чат зараз
Введення продукту

GNEE is a manufacturer, trader, stockist, supplier and exporter of EN 10210 S355NH Carbon Steel Pipe. We offer steel pipes produced using the highest quality standards and focus on on-time delivery of orders through our efficient logistics management.
EN 10210 S355NH Seamless Pipe is made of iron and carbon materials. There are also welded and electric resistance welded pipe types. It has a content of 0.2% carbon, 1.6% manganese, silicon, phosphorus and sulfur. This elemental composition gives EN 10210 S355NH Low Carbon Pipe a minimum yield strength of 355MPa and a minimum tensile strength of 630MPa.
EN 10210 S355NH Black Steel Pipe has a dull appearance similar to a matte finish. Applications include corrosive high temperature and high pressure environments such as oil and gas industry, structural engineering and building frameworks.

sales@gneetube.com
 

EN1021 S355NH Seamless Steel Pipe Product specification

EN 10210 S355NH Tubes Grade Standard And Specification

S355NH
6000-14000 mm
BS EN 10210
Black, Varnish/Oil Coating, Pre-Galvanized, Hot Dip Galvanized
21.3-914mm
0.5mm - 25mm

EN 10210 S355NH Hydraulic Pipe Chemical Properties

0.23 max 0.05 max 1.60 max 0.05 max 0.05 max

EN 10210 S355NH Structural Pipe Mechanical Properties

Elongation A5 min
355 50,000 470 630

EN 10210 S355NH Black Seamless Steel Pipe Equivalent Designation

DIN -17124 Grade FGS 36 EN 10210-1 Grade S355NH NFA 49-501 Grade TU E355 ASTM A 500 Grade C ASME SA 500 Grade C

Carbon Steel EN 10210 S355NH Seamless Pipe 

EN 10210 S355NH High Temperature Pipe

Gnee has 14 steel production lines, 10 processing equipment for processing, bending, painting, heat treatment, cutting, drilling, beveling, tempering, surface treatment, complete testing equipment and strong technical force. The annual production capacity is more than 60,000 tons.

EN10210 S355NH Carbon Steel Pipe

1.One-Stop Solution

2.Competitive Price

3.Quick Shipping

4.Quality Control

 

Популярні Мітки: en10210 s355nh carbon steel pipe, China en10210 s355nh carbon steel pipe manufacturers, suppliers, factory

Послати повідомлення

whatsapp

Телефон

Електронна пошта

Розслідування